Cracks often start at the entry or exit point of a cut because that is where the heat dwells the longest.

Use SheetCam’s Optimization settings. Instead of cutting the "closest next" part, you can manually sequence the cuts or use a "keep cool" strategy. By jumping the torch to different areas of the sheet, you allow the material to dissipate heat, keeping the overall temperature of the HAZ below the critical cracking threshold. 4. Cutting Speed and Feed Rates

While often associated with the welding process, hot cracking in the context of SheetCam and CNC plasma cutting refers to the structural failure or "tearing" of the metal during or immediately after the thermal cycle of the cut.

Use a "Leadin Type" of Arc in your operation settings. This provides a smoother transition for the plasma arc, reducing the sudden thermal shock to the boundary layer of the part. 2. Path Rules and "Overburn"